Well after about two and half weeks, it was time to do some level sanding and a polish. Again, familiar territory for Pitbullers so I didn't take many pics. Wet sanded with 1000, until it was level (ish) and then carried on gently with 1500, 2000 and 2500.
I've used Farecla products before on boats and found them ok, so I broke out Amazon again and purchased some Farecla G10 finishing compound, which came with a buffing pad that fitted on my sander, Started off gently then increased the speed a bit and ended up with a fairly nice finish (in my opinion). Little bit glossier than I was going for, but glass smooth to the touch.