Results 1 to 10 of 15

Thread: TLA-1 Build

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Quote Originally Posted by McCreed View Post
    Just curious, did you reapply the grain filler after sanding back the stain?
    Oooh - no, I didn't. Does sanding back dig out some of the grain?

  2. #2
    Overlord of Music McCreed's Avatar
    Join Date
    Oct 2018
    Location
    AUS
    Posts
    3,552
    Quote Originally Posted by Johnny Bravo View Post
    Oooh - no, I didn't. Does sanding back dig out some of the grain?
    If you were sanding with a grit like P240 or coarser in an effort to remove stained timber, that aggregate would also be larger enough to remove grain filler IMO.
    Making the world a better place; one guitar at a time...

  3. #3
    Quote Originally Posted by McCreed View Post
    If you were sanding with a grit like P240 or coarser in an effort to remove stained timber, that aggregate would also be larger enough to remove grain filler IMO.
    That makes a lot of sense.

    Well that is definitely a lesson learned because when I went to wet sand my acrylic top coat, the sanded material settled into the grain and then I had to find a way to get that out. Cutting compound wouldn't do it but more wet sanding compounded the problem. In the end i tried a little acetone but in my enthusiasm i burnt through a small patch.

    Many of the swear words were said....

    Sent from my SM-G930F using Tapatalk