Quote Originally Posted by wazkelly View Post
Dedman's advice is spot on.

Give the steel wool away as that stuff can break down into small particles that get trapped in subsequent finish coats.

1200 wet light wet sand after 8 - 10 coats then 1500 after 12 - 15 and stepping up to 2000 from there until really happy with things.

Sent from my SM-A520F using Tapatalk
Shielding paint is best done last after fully polished and need to mask off to prevent getting some on anywhere it is not meant to go.

Sent from my SM-A520F using Tapatalk