Dedman's advice is spot on.
Give the steel wool away as that stuff can break down into small particles that get trapped in subsequent finish coats.
1200 wet light wet sand after 8 - 10 coats then 1500 after 12 - 15 and stepping up to 2000 from there until really happy with things.
Sent from my SM-A520F using Tapatalk