    Quote Originally Posted by Bluesmartyboy View Post
    Would you do a few neat coats of TO followed by a wet sand to pore fill then repeat the coat and wet sand route and if so,
    Although I haven't tried this method, I've read that a good idea is to apply the first coat of TO with (I think...) 600 grit W&D. [EDIT! I found the video - it's actually 1200 grit.]

    This works as a grain/scratch filler as the first TO coat takes on the colour of the finish.

    Like I said, I haven't tried this method yet, but I intend to with my first build. I'm still only at the intensifier stage at the moment, so watch this space...
    Last edited by Muzza; 01-04-2016 at 08:33 AM.
    first build PRS-1TS in progress...
    http://www.buildyourownguitar.com.au...ead.php?t=4937

    second build PRS-1Q in progress...
    http://www.buildyourownguitar.com.au...ead.php?t=4956

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •