I usually aim for around 20+ Tru-oiil coats, 10 full strength and then 10 at 50/50 with white spiriits. If you're wet sanding after every coat then you're gettng minimal build up of thickness, so more would be better.
I usually aim for around 20+ Tru-oiil coats, 10 full strength and then 10 at 50/50 with white spiriits. If you're wet sanding after every coat then you're gettng minimal build up of thickness, so more would be better.
Scott.
Thanks guys, ive only done 2 sands with 1200 grit one at coat 5 and 9 and i layed it on fairly thick . I thought the t/o was oil based not spirit based
It is, but white spirit will still thin it and evaporate away.
... and not swell the wood like a normal water 'wet' sand will.
Scott.
Did some dt wax on the fret board tonight and it has come up sweet, plus a thinned out coat of oil, i think i will only need a lambswool pad to buff its that shiny and smooth, another 2 or 3 coats and it will look like glass.
The photos dont really show the quilted maple, as you walk around it the pattern changes to watch it become more pronounced after each coat ita hard to describe
As per Weirdy I'd go 20+ coats of tru oil. You'll just know when enough is enough it will suddenly start looking nice and glassy with some depth to it (if that's the look you are going for)
Sent from my iPhone using Tapatalk
Current Projects