Good advice from Andy, particularly with 2000 wet sand between each coat as any coarser will strip it in no time as DT can tend to be quite soft.
On my first build I had an oh dear moment after using 0000 steel wool (and as a result never used that crap again since) and wet sanded with around 600 or 800 and in a blink went through to bare timber in a few spots and right through most layers of intensifier in others. Plenty of swear words but more due to the loss of colour and the time and effort required to bring it back to the same standard.
Best to take things very slow and carefully with DT, a bit like the hare and the tortoise as quick will most likely take longer to cure and finish overall.