That does look rather nice. Bushfire Sunrise or Coolangatta Gold?
If you splash similar number of coats on scrap timber and then add 1 intensifier you will see what difference it makes.
Hard to describe and similar to the prescence control on an amp where somehow things are enhanced ever so slightly and in a good way.
Sent from my SM-A520F using Tapatalk
-
Outback Sunset. It’s very nice.
Understood. We’ll think about it, then.
Mostly I was just checking whether any parts were essential for proper operation of the finishes and/or solvents.
-
No, once you see the colour where you want it to be you can move on to final finishing.
Intensifier does enhance and adds a bit more 'zing' but not required as part of the curing process.
Sent from my SM-A520F using Tapatalk
-
-
If you’re doing Tru oil you don’t use the top coat
-